Metal Roof Coating for Leaking IBR Roofs: A Guide for Factory and Warehouse Managers

A metal roof coating is often the most practical fix for a leaking IBR roof on a factory or warehouse, as long as the sheets are still sound. Most leaks on these roofs start at the laps, fasteners and flashings, not in the open sheet. So the job is to seal those details first, then cover the whole roof in one continuous silicone membrane. This guide is for the facilities or maintenance manager who has to choose between patching again, reroofing or coating.

Why IBR roofs start leaking

Installers fix IBR and corrugated sheeting with screws through the crest, and every screw is a hole with a washer over it. Over the years those washers harden in the sun. At the same time, the sheets expand and contract every day, so screws work loose and water finds the gap. Laps are the next weak point. Because the sheets only overlap, wind driven rain pushes water up under the lap and capillary action draws it further in.

On the coast the problem speeds up. Salt air settles in the laps and around the screw heads, and those spots stay damp long after the open sheet has dried. As a result, rust usually starts at cut edges, laps and fasteners while the rest of the sheet still looks fine. That pattern matters, because it means most of the roof is still worth keeping.

Repair, reroof or apply a metal roof coating?

Patching with mastic or tape fixes one leak at a time, and the next leak often shows up a metre away. Reroofing fixes everything, but it means stripping sheets over a working building and buying new steel and fasteners. A coating sits between the two. The existing sheets stay in place, so the building stays closed while the work goes on.

In practice the decision comes down to the condition of the steel. First, have someone walk the roof safely and look at the laps, fasteners and gutters. If most sheets show only surface rust and rust at the details, coating makes sense. However, where sheets are holed or flaking right through over large areas, replace those sheets first. A coating bridges small gaps at laps and screws, but it is not a structural repair for steel that has lost its thickness.

How a silicone metal roof coating goes on

The product we supply for this work is SI-COAT 461 RC, a 100% silicone, moisture cure roof coating with 94% volume solids. The work follows four steps.

First, clean the roof. CSL asks for a power wash with a suitable detergent and a rinse. CSL 471 concentrated roof cleaner suits this step. Then remove all loose rust, loose mill scale, old sealant and flaking paint by wire brushing or power tool cleaning. Let the roof dry fully before anything goes on.

Second, do an adhesion test patch. CSL recommends one on every metal roof and on any roof with an existing coating. No primer is needed on most common substrates, but the patch is how you prove that on your roof.

Third, seal the laps, fasteners and flashings, as described in the next section.

Finally, apply the coating, usually by airless spray. The applicator builds full thickness in a single coat, with wet on wet passes before the first pass skins. Brush and roller need more passes, again wet on wet in the same session. The target is at least 0.5 mm once dry (20 mil, 508 µm), which is roughly half a litre per m² before losses. Theoretical coverage is about 2.1 m²/L at 18 mil and 1.7 m²/L at 22 mil. So add a loss factor, and remember that profiled sheeting has more surface area than its plan area.

Conditions matter too. The surface must be between 5°C and 60°C and at least 3°C above the dew point. On coastal sites that often rules out early mornings, when the sheets are wet with dew. At 25°C and 50% RH, SI-COAT 461 RC skins in about 68 minutes and is dry in 4 to 6 hours. Full properties take 7 days.

Sealing laps, fasteners and flashings first

The details are where IBR roofs leak, so they get their own treatment before the main coat. CSL makes two silicone products for this. CSL lists CSL 463 roof sealant for metal roof seams, flashings, fasteners and drains. In addition, CSL 465 flashing sealant contains reinforcing material, and CSL lists it for fasteners, seams and pipe penetrations on metal roofs. Spread it at least 100 mm onto the roof around each detail, then top coat with SI-COAT 461 RC once it is dry to touch.

In practice that means every screw head, the end laps, the side laps, ridge and barge flashings, and every pipe through the roof. Also replace screws that have rusted badly or no longer hold. Because both sealants are neutral cure and compatible with the coating, the details and the open sheet form one continuous membrane.

Heat, salt air and daily movement

Steel sheets move between a hot afternoon and a cool night. The cured silicone stays flexible through that, with 282% elongation at 23°C and 330% at minus 18°C. It is also stable from minus 60°C to 200°C. That is why a silicone metal roof coating does not crack at the laps the way a rigid coating can. For a side by side view of the chemistries, see our comparison of acrylic, polyurethane and silicone roof coatings.

White SI-COAT 461 RC reflects the sun as well. Its CRRC listing (product ID 1368-0002) gives an initial solar reflectance of 0.856 and thermal emittance of 0.89, for an SRI of 107.9. After soiling, the figures are 0.723 and an SRI of 88.9. In a CSL case study the inside of the building ran 7 to 9°C cooler after coating. On an uninsulated factory, the people working below notice that. Our article on heat reflective roof coating covers this in more detail.

CSL designed the coating as a barrier against weathering, ageing and UV. It also withstands ponding water, which helps on low pitch sections where water lies after rain. Our article on ponding water on flat roofs explains why that matters. If you manage several sites, our articles cover the same approach for warehouses and shopping centres and for mine buildings.

Where a metal roof coating is the wrong answer

  • First, where sheets are rusted through over large areas or purlins are failing, replace the steel before you coat anything.
  • Also, SI-COAT 461 RC is not for asphalt shingles, and it is not for contact with potable water.
  • On mixed roofs, bitumen and torch on membranes always need CSL 468 epoxy primer first.
  • Then there is the weather, because the coating should not go onto a wet or dewy roof, or below 5°C.
  • Finally, a wet silicone roof is slippery, so plan walkways to plant and gutters with Si-COAT 462 RC walkpad.

Frequently asked questions

Does a metal roof coating need a primer?

Usually not. SI-COAT 461 RC needs no primer on most common substrates, including metal. Still, CSL asks for an adhesion test patch on every metal roof, so do one first. If the result is poor, CSL will advise a compatible primer. Our SI-COAT 461 FAQ answers more substrate questions.

How long does the coating take to cure?

At 25°C and 50% RH it skins in about 68 minutes and is dry in 4 to 6 hours. Full properties take 7 days. So plan the work for a dry spell, and keep foot traffic off the new coating.

Can the building stay in use while the roof is coated?

In most cases, yes. Because the sheets stay in place, the building stays closed and the work happens on the outside. However, agree on overspray control near vents, vehicles and neighbouring roofs before spraying starts.

Will the coating stop the sheets rusting?

It forms a waterproof layer over the steel, so rain and salt no longer sit in the laps and around the screws. But it cannot restore steel that has already rusted through. That is why loose rust comes off first and holed sheets get replaced. For rusting steel structures other than roofs, read our guide to corrosion protection methods.

How long will a metal roof coating last?

CSL reports SI-COAT 461 RC roofs in service in North America for more than 20 years. When the roof needs attention again, you can recoat silicone with silicone, with no tear off. You can also see how CSL coatings have held up on other plants on our case studies page.

Technical Solution Supplies distributes CSL Silicones products across Southern Africa, including the DRC and the Seychelles. To check whether your roof suits a coating, send us photos of the laps, fasteners and gutters through our contact page.

Proud exclusive distributor of CSL Silicones in Southern Africa.

Leave a Comment